BRT-500B مقياس السعرات الحرارية بالمسح التفاضلي (DSC) يتوافق بدقة مع ISO 11357, جيجابايت/ت 19466, and ASTM D3418 standards. Powered by a dual temperature probe system with 0.01 mW / 0.01 °C resolution, it features automated N2/O2 gas switching, a 7-inch color touchscreen, a adhesive-free closed furnace (RT–500 °C), and auto-calibration for measuring Tg, melting point, enthalpy, and Oxidation Induction Time (OIT).
ال BRT-500B مقياس السعرات الحرارية بالمسح التفاضلي (DSC) is a high-precision laboratory thermal analysis system engineered strictly in accordance with ايزو 11357, جيجابايت/ت 19466, ASTM D3418, و ASTM E1356 المعايير. Designed for polymer chemistry, pharmaceutical R&D, rubber testing, and industrial quality control laboratories, it evaluates critical phase transitions, heat capacity changes, and thermal oxidation stability across thermoplastics, resins, المركبات, and organic compounds.
Equipped with an advanced dual temperature probe architecture and a dynamic DSC measuring range of 0 to ±500 mW (0.01 mW / 0.01 °C resolution), هذا المسح التفاضلي المسعر (DSC) measures glass transition temperature (Tg), melting point, cold crystallization, curing enthalpy, and Oxidation Induction Time (OIT). Featuring automated N2 and O2 dual-gas switching, an industrial 7-inch LCD touchscreen, and a fully enclosed mechanical furnace that eliminates interior adhesive contamination, the BRT-500B delivers certified analytical repeatability from room temperature to 500 درجة مئوية.
المسح التفاضلي المسعر (DSC) المعايير
This optical thermal analysis system enables certified laboratories to assess thermodynamic behavior in full compliance with global fire, polymer, and chemical testing standards:
| الكود القياسي | العنوان القياسي & نِطَاق | تطبيق الاختبار الأساسي |
|---|---|---|
| ايزو 11357 (Parts 1–6) | Plastics — Differential scanning calorimetry (DSC) general principles, Tg, melting, Cp & OIT | International core benchmark for comprehensive polymer thermal behavior analysis |
| جيجابايت/ت 19466 (Parts 1–6) | Plastics — Differential scanning calorimetry (DSC) standard methods | Mandatory Chinese national standard for thermal analysis of plastics and resins |
| ASTM D3418 / ASTM E1356 | Standard Test Method for Transition Temperatures and Enthalpies of Polymers by DSC | North American standard for glass transition, melting, and crystallization testing |
Technological Features of BRT-500B Differential Scanning Calorimeter (DSC)
- Dual Temperature Probe System
Employs one independent probe dedicated to furnace PID heating control while a second high-precision thermocouple measures sample temperature directly. This arrangement eliminates thermal lag and records accurate Tg and reaction kinetics.
- Ultra-High Precision Resolution (0.01 درجة مئوية / 0.01 mW)
Features a dynamic heat flow range of 0 to ±500 mW with 0.01 mW sensitivity alongside 0.01 °C temperature display resolution, ensuring clean baseline stability for subtle endothermic and exothermic events.
- Automated Dual-Gas Switching Mechanism (ن2 / O2)
Integrates automatic nitrogen and oxygen gas switching with digital flow control (0–200 mL/min). Facilitates seamless transitions between inert purging and oxidative atmospheres required for standardized OIT evaluations.
- Fully Enclosed Contamination-Free Furnace Structure
Eliminates internal colloids and organic adhesives through pure mechanical fixing, preventing high-temperature outgassing contamination. The closed bracket design prevents debris from falling into the heating chamber.
- Self-Calibration Standard & Interactive Interface
Supplied with certified Indium (في), Tin (Sn), and Zinc (Zn) pure reference materials for rapid multi-point temperature and enthalpy calibration via the 7-inch 24-bit color LCD touch screen.
Technical Specifications of Differential Scanning Calorimeter (DSC)
| نموذج المنتج | BRT-500B مقياس السعرات الحرارية بالمسح التفاضلي (DSC) |
| Temperature Range & دقة | درجة حرارة الغرفة إلى 500 درجة مئوية; Temperature Resolution: 0.01 درجة مئوية |
| Heating & Cooling Ramping Rates | Heating Rate: 0.1 ل 80 °C/min; Cooling Rate: 0.1 ل 30 °C/min |
| DSC Measuring Range & Sensitivity | Dynamic Range: 0 to ±500 mW; دقة: 0.01 mW; Sensitivity: 0.1 mW |
| التحكم في غازات الجو | Nitrogen (ن2) & Oxygen (O2); Auto-switching; Pressure: 0.2 MPa; Flow: 0–200 mL/min |
| Sample Crucible Type | Standard Uncovered Aluminum Crucible (Φ6.5 × 3 مم) |
| Calibration Reference Standards | Pure Indium (في), Tin (Sn), and Zinc (Zn) included for temperature & enthalpy adjustment |
| Furnace & Power Requirements | Fully enclosed mechanical bracket structure; تيار متردد 220 فولت, 50 هرتز (300W total power) |
System Architecture & Applications of Differential Scanning Calorimeter (DSC)
سير عمل الاختبار الموحد:
- Weigh the test sample (typically 5–10 mg) into a standard aluminum crucible and place it onto the sample platform alongside the reference pan inside the heating chamber.
- Select the target thermal method (على سبيل المثال, dynamic heating ramp, isothermal hold, or dynamic OIT method) on the touch screen or PC software interface.
- Set the purge gas parameters (N2 for thermal transitions, switching to O2 at specified isothermal temperatures for OIT evaluations).
- Initiate the scan; the dual temperature probes and heat flow sensors capture thermal transitions in real time, plotting precise differential power curves.
- Use the software toolset to calculate glass transition inflection points (Tg), peak melting/crystallization temperatures, area enthalpy integrals, and oxidation onset times.
تطبيقات العملاء المستهدفة:
- Thermoplastic resin compounding, masterbatch, and synthetic rubber manufacturing facilities.
- Polymer insulation, automotive composite parts, and packaging material quality control labs.
- Pharmaceutical solid-state analysis, chemical synthesis, and energetic material research centers.
- University material science departments, polymer engineering labs, and third-party testing institutes.
المسح التفاضلي المسعر (DSC) التعليمات
س1: How does the dual temperature probe system improve testing accuracy?
أ: One probe regulates the furnace wall temperature via PID control, while the second probe rests directly beneath the sample pan. This dual configuration compensates for thermal lag and records the true real-time sample response, delivering highly accurate Tg and peak enthalpy data.
Q2: Can the BRT-500B measure Specific Heat Capacity (Cp) and Oxidation Induction Time (OIT)?
أ: نعم. OIT testing (both isothermal and dynamic) is fully supported out of the box per ISO 11357-6. Specific Heat Capacity (Cp) testing per ISO 11357-4 is available via an optional software and hardware expansion module.
س3: Why is the adhesive-free furnace structure important for high-temperature testing?
أ: Traditional heating chambers assembled with organic glues can outgas or degrade when heated above 300 درجة مئوية, generating baseline drift and false thermal peaks. The BRT-500B mechanical-fixation furnace eliminates glues entirely, preserving baseline stability across the entire 500 °C temperature range.












التعليقات
لا توجد تعليقات حتى الآن.